Purpose:
General purpose flame-retardant steel cord conveyor belt is suitable for material conveying in coal washing plant, power plant and non coal underground mining. It is suitable for conveying massive, granular and powder materials in high strength, long distance and large volume.
Structure:
General purpose flame retardant steel cord conveyor belt is composed of upper covering layer, lower covering layer, steel wire rope, adhesive layer and side glue.
Features:
This product has the characteristics of general flame-retardant, high tensile strength, impact resistance, good elasticity, high wear resistance, small elongation, good adhesion between rubber and steel wire rope, even tension of steel wire rope, good slotting performance, etc. it is suitable for conveying massive, granular and powdery materials under the occasions of high strength, long distance and large transportation volume.
·Executive standard: Hg / T 3973-2007 general purpose flame retardant steel cord conveyor belt
Main technical indicators:
and strength | Tensile strength | A wire rope | A wire rope | Thickness of upper and lower overburden | A wire rope | Adhesion strength of steel wire rope ≥ | |
Before aging | After aging | ||||||
ST-630 | 630 | 10 | 3.0 | 5+5 | 6.93 | 60 | 55 |
ST-800 | 800 | 10 | 3.5 | 5+5 | 8.8 | 70 | 65 |
ST-1000 | 1000 | 12 | 4.0 | 6+6 | 13.2 | 80 | 75 |
ST-1250 | 1250 | 12 | 4.5 | 6+6 | 16.5 | 95 | 90 |
ST-1600 | 1600 | 12 | 5.0 | 6+6 | 21.12 | 105 | 95 |
ST-2000 | 2000 | 12 | 6.0 | 8+6 | 26.4 | 105 | 95 |
ST-2500 | 2500 | 15 | 7.2 | 8+6 | 41.25 | 130 | 120 |
ST-2800 | 2800 | 15 | 7.6 | 8+6 | 45.9 | 135 | 125 |
ST-3150 | 3150 | 15 | 8.1 | 8+8 | 51.98 | 140 | 130 |
ST-3500 | 3500 | 15 | 8.6 | 8+8 | 57.7 | 145 | 140 |
ST-4000 | 4000 | 15 | 8.9 | 8+8 | 66.0 | 150 | 145 |
ST-4500 | 4500 | 16 | 9.7 | 8+8 | 79.2 | 165 | 160 |
ST-5000 | 5000 | 17 | 10.9 | 8.5+8.5 | 93.5 | 175 | 170 |
ST-5400 | 5400 | 17 | 11.3 | 9+9 | 101 | 180 | 175 |
Item | Type | |||
H(Strong splitting) | D(Strong wear) | L(General conditions) | ||
Tensile strength of overburden / MPa ≥ | 20 | 18 | 15 | |
Elongation at break of coating / % ≥ | 400 | 400 | 350 | |
Wear volume / mm3 ≤ | 200 | 120 | 200 | |
Aging test (70 ℃× 168h) | ±25% | |||
Adhesion strength between cover layer and core layer,≥N/mm | 12 | |||
K2 | K3 | |||
Flame duration | The total flame duration of 6 samples with covering layer shall not be more than 45s, and any single value shall not be more than 15s. | The average value of flame duration of three samples with cover layer shall not be greater than 60s. | ||
Electrostatic conductivity | ≤3 × 108 Ω | |||
Reburning property | There shall be no re emergence of flame on any one of the test pieces. |
Purpose:
General purpose flame-retardant steel cord conveyor belt is suitable for material conveying in coal washing plant, power plant and non coal underground mining. It is suitable for conveying massive, granular and powder materials in high strength, long distance and large volume.
Structure:
General purpose flame retardant steel cord conveyor belt is composed of upper covering layer, lower covering layer, steel wire rope, adhesive layer and side glue.
Features:
This product has the characteristics of general flame-retardant, high tensile strength, impact resistance, good elasticity, high wear resistance, small elongation, good adhesion between rubber and steel wire rope, even tension of steel wire rope, good slotting performance, etc. it is suitable for conveying massive, granular and powdery materials under the occasions of high strength, long distance and large transportation volume.
·Executive standard: Hg / T 3973-2007 general purpose flame retardant steel cord conveyor belt
Main technical indicators:
and strength | Tensile strength | A wire rope | A wire rope | Thickness of upper and lower overburden | A wire rope | Adhesion strength of steel wire rope ≥ | |
Before aging | After aging | ||||||
ST-630 | 630 | 10 | 3.0 | 5+5 | 6.93 | 60 | 55 |
ST-800 | 800 | 10 | 3.5 | 5+5 | 8.8 | 70 | 65 |
ST-1000 | 1000 | 12 | 4.0 | 6+6 | 13.2 | 80 | 75 |
ST-1250 | 1250 | 12 | 4.5 | 6+6 | 16.5 | 95 | 90 |
ST-1600 | 1600 | 12 | 5.0 | 6+6 | 21.12 | 105 | 95 |
ST-2000 | 2000 | 12 | 6.0 | 8+6 | 26.4 | 105 | 95 |
ST-2500 | 2500 | 15 | 7.2 | 8+6 | 41.25 | 130 | 120 |
ST-2800 | 2800 | 15 | 7.6 | 8+6 | 45.9 | 135 | 125 |
ST-3150 | 3150 | 15 | 8.1 | 8+8 | 51.98 | 140 | 130 |
ST-3500 | 3500 | 15 | 8.6 | 8+8 | 57.7 | 145 | 140 |
ST-4000 | 4000 | 15 | 8.9 | 8+8 | 66.0 | 150 | 145 |
ST-4500 | 4500 | 16 | 9.7 | 8+8 | 79.2 | 165 | 160 |
ST-5000 | 5000 | 17 | 10.9 | 8.5+8.5 | 93.5 | 175 | 170 |
ST-5400 | 5400 | 17 | 11.3 | 9+9 | 101 | 180 | 175 |
Item | Type | |||
H(Strong splitting) | D(Strong wear) | L(General conditions) | ||
Tensile strength of overburden / MPa ≥ | 20 | 18 | 15 | |
Elongation at break of coating / % ≥ | 400 | 400 | 350 | |
Wear volume / mm3 ≤ | 200 | 120 | 200 | |
Aging test (70 ℃× 168h) | ±25% | |||
Adhesion strength between cover layer and core layer,≥N/mm | 12 | |||
K2 | K3 | |||
Flame duration | The total flame duration of 6 samples with covering layer shall not be more than 45s, and any single value shall not be more than 15s. | The average value of flame duration of three samples with cover layer shall not be greater than 60s. | ||
Electrostatic conductivity | ≤3 × 108 Ω | |||
Reburning property | There shall be no re emergence of flame on any one of the test pieces. |